Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 92.0 - 95.0 °C | 198 - 203 °F | after thermal post treatment procedure B; ASTM D648-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 95.0 °C | 194 - 203 °F | |
Reliance Industries Polypropylene Random Copolymer Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 95.0 °C | 149 - 203 °F | Average value: 71.2 °C Grade Count:14 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 95.0 °C | 194 - 203 °F | |
C.O.I.M. EXTER S® S 101 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 101: Medium/high rea.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 95.0 °C | 194 - 203 °F | |
C.O.I.M. EXTER S® S 104 L Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 104 L: Same performa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 95.0 °C | 194 - 203 °F | |
C.O.I.M. EXTER S® S 201 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 201: Polyester resin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 68.0 - 95.0 °C | 154 - 203 °F | Average value: 81.7 °C Grade Count:41 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |