Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.0 - 427 °C |
6.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.0 - 427 °C |
6.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 27.0 - 204 °C |
6.50 µin/in-°F @Temperature 80.6 - 399 °F |
|
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 300 °C |
6.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Deloro® 50 Nickel Alloy Nickel base. Provides maximum amount of abrasion and metal-on-metal wear resistance for cast components. Superior wear resistance. Adequate corrosion resistance. Tungsten carbide tools allow for mac.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 500 °C |
6.50 µin/in-°F @Temperature 932 °F |
upon cooling |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 1000 °C |
6.50 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 1000 °C |
6.50 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec MZ 429 Zirconia, ZrO2-Y2O3 MZ 429 is a yttria-stabilized zirconia ceramic. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 399 °C |
6.50 µin/in-°F @Temperature 68.0 - 750 °F |
|
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 0.000 - 649 °C |
6.50 µin/in-°F @Temperature 32.0 - 1200 °F |
|
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 0.000 - 649 °C |
6.50 µin/in-°F @Temperature 32.0 - 1200 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.1 - 260 °C |
6.50 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 500 °C |
6.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 200 °C |
6.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.Applications: Taps, twist drills, reamers, broaching tools, meta.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 200 °C |
6.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 800 °C |
6.50 µin/in-°F @Temperature 68.0 - 1470 °F |
|
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL) |
|||
CTE, linear | 11.7 µm/m-°C @Temperature <=427 °C |
6.50 µin/in-°F @Temperature <=801 °F |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.1 - 204 °C |
6.50 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; .. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
Annealed |
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 200 °C |
6.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 500 °C |
6.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |