Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 100 - 115 µm/m-°C @Temperature 25.0 - 200 °C |
55.6 - 63.9 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
CTE, linear | 70.0 - 115 µm/m-°C @Temperature 25.0 - 100 °C |
38.9 - 63.9 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM D696 |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |