Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
ISO 11359 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ASTM D696 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=152 °C |
25.0 µin/in-°F @Temperature <=306 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature >=149 °C |
25.0 µin/in-°F @Temperature >=300 °F |
ASTM E228 |
Greene Tweed Arlon® 1163 PEEK, Glass Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
Alpha 1 |
Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive TRA-BOND 226U01 is a one-part, controlled flow adhesive with high temperature resistance.Information provided by Tra-Con Inc. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature 50.0 - 200 °C |
25.0 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature 200 - 300 °C |
25.0 µin/in-°F @Temperature 392 - 572 °F |
DIN 53 752 |
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
CTE, linear | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6500-PMF Electrically conductive epoxy adhesive High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic d.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=28.0 °C |
25.0 µin/in-°F @Temperature <=82.4 °F |
below Tg |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=27.0 °C |
25.0 µin/in-°F @Temperature <=80.6 °F |
below Tg |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ISO 11359 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear | 45.0 µm/m-°C @Temperature <=143 °C |
25.0 µin/in-°F @Temperature <=289 °F |
Average below Tg; ASTM D696 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |