Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
across grain
Pyrotek PT-10 Graphite
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A..
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 100 °C
2.50 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1705 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 4.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KZFSN5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 4.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.50 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-ZK7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 4.50 - 6.50 µm/m-°C

@Temperature 20.0 - 300 °C
2.50 - 3.61 µin/in-°F

@Temperature 68.0 - 572 °F
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â..
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 600 °C
2.50 µin/in-°F

@Temperature 68.0 - 1110 °F
DIN EN 821-1
CeramTec CD 101 Silicon Carbide, SiC-ZrB2
CD101 is a zirconia reinforced silicon carbide designed for maximum hardness.
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 1000 °C
2.50 µin/in-°F

@Temperature 68.0 - 1830 °F
DIN EN 821-1
CeramTec CD 101 Silicon Carbide, SiC-ZrB2
CD101 is a zirconia reinforced silicon carbide designed for maximum hardness.
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 600 °C
2.50 µin/in-°F

@Temperature 68.0 - 1110 °F
DIN EN 821-1
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 100 °C
2.50 µin/in-°F

@Temperature 68.0 - 212 °F
ASTM-C372
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 100 °C
2.50 µin/in-°F

@Temperature 68.0 - 212 °F
ASTM-C372
CeramTec Rubalit® 702 Alumina, 85%
Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl..