Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.50 - 6.50 µm/m-°C @Temperature 20.0 - 300 °C |
2.50 - 3.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |