Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.46 g/cc
0.125 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 460
460
.1/20
Modulus of Elasticity 65.0 GPa
9430 ksi
Poissons Ratio 0.275
0.275
Shear Modulus 25.0 GPa
3630 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.50 µin/in-°F

@Temperature -22.0 - 158 °F
5.70 µm/m-°C

@Temperature 20.0 - 300 °C
3.17 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 501 °C
934 °F
Optical Properties Metric English Comments
Refractive Index 1.65412

@Wavelength 587.6 nm
1.65412

@Wavelength 587.6 nm
n<sub>d</sub>
1.65803

@Wavelength 546.1 nm
1.65803

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 93.7 %

@Thickness 10.0 mm,
Wavelength 380 nm
93.7 %

@Thickness 0.394 in,
Wavelength 380 nm
98 %

@Thickness 10.0 mm,
Wavelength 405 nm
98 %

@Thickness 0.394 in,
Wavelength 405 nm
99.4 %

@Thickness 10.0 mm,
Wavelength 460 nm
99.4 %

@Thickness 0.394 in,
Wavelength 460 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %

@Thickness 0.394 in,
Wavelength 580 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 24.6 %

@Thickness 10.0 mm,
Wavelength 2500 nm
24.6 %

@Thickness 0.394 in,
Wavelength 2500 nm
96.7 %

@Thickness 10.0 mm,
Wavelength 1530 nm
96.7 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 13 %

@Thickness 10.0 mm,
Wavelength 334 nm
13 %

@Thickness 0.394 in,
Wavelength 334 nm
51.5 %

@Thickness 10.0 mm,
Wavelength 350 nm
51.5 %

@Thickness 0.394 in,
Wavelength 350 nm
84.2 %

@Thickness 10.0 mm,
Wavelength 365 nm
84.2 %

@Thickness 0.394 in,
Wavelength 365 nm
88.7 %

@Thickness 10.0 mm,
Wavelength 370 nm
88.7 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 52.3
52.3
Alkali Class, AR 4.3
4.3
Stain Resistance Class, FR 2.0
2.0
Descriptive Properties Value Comments
B 1
Climatic Resistance Test CR 3
HG 5
K (10-6mm2/N) 2.89
Phosphate Resistance PR 4.3
T1013.0 (°C) 479
T107.6 (°C) 0