Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 °C |
2.50 µin/in-°F @Temperature 68.0 °F |
across grain |
Pyrotek PT-10 Graphite PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A.. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 100 °C |
2.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1705 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.50 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott KZFSN5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.50 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-ZK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 4.50 - 6.50 µm/m-°C @Temperature 20.0 - 300 °C |
2.50 - 3.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 600 °C |
2.50 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 1000 °C |
2.50 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 600 °C |
2.50 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 100 °C |
2.50 µin/in-°F @Temperature 68.0 - 212 °F |
ASTM-C372 |
CeramTec Rubalit® 600 Alumina, 48% Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors. |
|||
CTE, linear | 4.50 µm/m-°C @Temperature 20.0 - 100 °C |
2.50 µin/in-°F @Temperature 68.0 - 212 °F |
ASTM-C372 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |