Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe HS-105â„¢ ASTM M35 DIN 1.3243 High Speed Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name HS-105™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe HS-105â„¢ ASTM M35 DIN 1.3243 High Speed Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HS-105 high speed steel is a cobalt-modified M2 high speed steel in which the cobalt addition provides hot hardness that is intermediate between those of M2 and M42 high speed steels. The improved hot hardness makes the steel suitable for machining high-strength and prehardened steels, high-hardness alloys, and the difficult-to-machine, nonferrous superalloys used in the aerospace, oil, and power generation industries. Typical applications for HS-105 high speed steel include twist drills, taps, milling cutters, reamers, broaches, saws, knives, and hobs.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 8.14 g/cc
8.14 g/cc
Density 8.14 g/cc
0.294 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64.8
64.8
Oil Quenched from 1232°C, 5 minutes
65.2
65.2
Oil Quenched from 1177°C, 5 minutes
65.2
65.2
Oil Quenched from 1204°C, 5 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 45 - 50 %
45 - 50 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 11.4 µm/m-°C

@Temperature 21.0 - 399 °C
6.33 µin/in-°F

@Temperature 69.8 - 750 °F
11.5 µm/m-°C

@Temperature 21.0 - 593 °C
6.39 µin/in-°F

@Temperature 69.8 - 1100 °F
Component Elements Properties Metric English Comments
Carbon, C 0.93 %
0.93 %
Chromium, Cr 4.2 %
4.2 %
Cobalt, Co 4.9 %
4.9 %
Iron, Fe 76.52 %
76.52 %
Molybdenum, Mo 5.0 %
5.0 %
Silicon, Si 0.30 %
0.30 %
Tungsten, W 6.25 %
6.25 %
Vanadium, V 1.9 %
1.9 %
Chemical Properties Metric English Comments
Critical Temperature 849 °C
1560 °F
Ac1