Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel 430 Ferritic Stainless steel

Category Metal , Ferrous Metal , Ferritic , Stainless Steel , T 400 Series Stainless Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 430 Ferritic Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, furnace combustion chambers, dishwashers, range hoods, gas burners, gutters, steam iron bases and flatware. Industrial applications range from interior architectural applications to nitric acid plant equipment.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.74 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 85
85
Tensile Strength, Ultimate 483 MPa
70100 psi
Tensile Strength, Yield 310 MPa

@Strain 0.200 %
45000 psi

@Strain 0.200 %
Elongation at Break 25 %
25 %
in 2 inches
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 10.4 µm/m-°C

@Temperature 0.000 - 100 °C
5.78 µin/in-°F

@Temperature 32.0 - 212 °F
11.4 µm/m-°C

@Temperature <=538 °C
6.33 µin/in-°F

@Temperature <=1000 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 26.1 W/m-K

@Temperature 100 °C
181 BTU-in/hr-ft²-°F

@Temperature 212 °F
26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe >= 79.31 %
>= 79.31 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm
0.0000600 ohm-cm