Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.4 µm/m-°C @Temperature 450 °C |
5.78 µin/in-°F @Temperature 842 °F |
|
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 500 °C |
5.78 µin/in-°F @Temperature 932 °F |
upon cooling |
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 26.7 - 93.3 °C |
5.80 µin/in-°F @Temperature 80.0 - 200 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.80 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.80 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 20.0 - 95.0 °C |
5.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microst.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.80 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.78 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 20.0 - 98.9 °C |
5.80 µin/in-°F @Temperature 68.0 - 210 °F |
|
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.78 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature -17.8 - 37.8 °C |
5.80 µin/in-°F @Temperature 0.000 - 100 °F |
|
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.78 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 23.0 - 204 °C |
5.78 µin/in-°F @Temperature 73.4 - 399 °F |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 23.0 - 204 °C |
5.78 µin/in-°F @Temperature 73.4 - 399 °F |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.80 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |