Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.4 µm/m-°C @Temperature 26.7 - 93.3 °C |
5.80 µin/in-°F @Temperature 80.0 - 200 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.80 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 0.000 - 100 °C |
5.80 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.80 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 20.0 - 98.9 °C |
5.80 µin/in-°F @Temperature 68.0 - 210 °F |
|
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature -17.8 - 37.8 °C |
5.80 µin/in-°F @Temperature 0.000 - 100 °F |
|
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
CTE, linear | 10.4 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.80 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |