Crucible Steel AIRDI® 150 (AISI D2) Tool Steel

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel , Air-Hardening Steel
Manufacturer Crucible Steel
Trade Name AIRDI®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel AIRDI® 150 (AISI D2) Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microstructure. Airdi 150 (D2) has been widely used for many years in cold work applications requiring very high wear resistance. It is machinable in the annealed condition and, like other air-hardening tool steels, exhibits minimal distortion on hardening.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.695 g/cc
0.2780 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 221 - 225
221 - 225
Annealed
Hardness, Rockwell C 60 - 62
60 - 62
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 28.0 J
20.7 ft-lb
Austenitizing Temperature- 1010°C
Thermal Properties Metric English Comments
CTE, linear 10.4 µm/m-°C

@Temperature 20.0 - 95.0 °C
5.78 µin/in-°F

@Temperature 68.0 - 203 °F
11.3 µm/m-°C

@Temperature 20.0 - 205 °C
6.28 µin/in-°F

@Temperature 68.0 - 401 °F
12.6 µm/m-°C

@Temperature 20.0 - 540 °C
7.00 µin/in-°F

@Temperature 68.0 - 1000 °F
Thermal Conductivity 20.9 W/m-K

@Temperature 95.0 °C
145 BTU-in/hr-ft²-°F

@Temperature 203 °F
24.2 W/m-K

@Temperature 315 °C
168 BTU-in/hr-ft²-°F

@Temperature 599 °F
25.6 W/m-K

@Temperature 540 °C
178 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Shrinkage -0.0250 %

@Treatment Temp. 1010 °C
-0.0250 %

@Treatment Temp. 1850 °F
Hardening
Component Elements Properties Metric English Comments
Carbon, C 1.55 %
1.55 %
Chromium, Cr 11.5 %
11.5 %
Iron, Fe 85.25 %
85.25 %
As Remainder
Molybdenum, Mo 0.90 %
0.90 %
Vanadium, V 0.80 %
0.80 %