Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 500 °C |
5.61 µin/in-°F @Temperature 77.0 - 932 °F |
|
Osprey Metals CE9 Al-Si Controlled Expansion Alloy Si-40%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 700 °C |
5.61 µin/in-°F @Temperature 1290 °F |
|
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 250 °C |
5.61 µin/in-°F @Temperature 482 °F |
upon cooling |
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 21.0 - 204 °C |
5.61 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 300 °C |
5.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG12 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 500 °C |
5.61 µin/in-°F @Temperature 68.0 - 932 °F |
|
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 0.000 - 316 °C |
5.60 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 0.000 - 316 °C |
5.60 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 0.000 - 315 °C |
5.61 µin/in-°F @Temperature 32.0 - 599 °F |
|
Crucible Steel 416R Chromium Stainless Steel Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific req.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 30.0 - 800 °C |
5.61 µin/in-°F @Temperature 86.0 - 1470 °F |
|
Ametek Molybdenum-Copper Composite AMC 6436 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 316 °C |
5.61 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 400 °C |
5.61 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 400 °C |
5.61 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 400 °C |
5.61 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 400 °C |
5.61 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 21.0 - 93.0 °C |
5.61 µin/in-°F @Temperature 69.8 - 199 °F |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 100 °C |
5.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 25.0 - 400 °C |
5.61 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
CTE, linear | 10.1 µm/m-°C @Temperature 20.0 - 300 °C |
5.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG25 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |