Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 843°C

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name Hiperco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 843°C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core loss. This alloy is produced in strip form only and contains a small niobium addition for grain refinement during mill processing and final heat treatment of strip.Hiperco alloy 50 strip has been used primarily in the manufacture of rotor and stator laminations in motors and generators for aircraft power generation applications. These laminations are stamped from cold rolled strip and must be final annealed in a protective atmosphere or vacuum environment at a temperature which will provide and optimum combination of mechanical and magnetic properties to withstand the high stresses encountered in service.Hiperco 50 has the same nominal composition as Vanadium Permendur and Permendur V.Hiperco® is a registered trademark of Carpenter Technology Corporation. Data provided by Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 8.12 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 813 MPa
118000 psi
Tensile Strength, Yield 434 MPa

@Strain 0.200 %
62900 psi

@Strain 0.200 %
Elongation at Break 9.0 %
9.0 %
in 50 mm
Modulus of Elasticity 207 GPa
30000 ksi
Thermal Properties Metric English Comments
CTE, linear 9.50 µm/m-°C

@Temperature 25.0 - 200 °C
5.28 µin/in-°F

@Temperature 77.0 - 392 °F
10.1 µm/m-°C

@Temperature 25.0 - 400 °C
5.61 µin/in-°F

@Temperature 77.0 - 752 °F
10.5 µm/m-°C

@Temperature 25.0 - 600 °C
5.83 µin/in-°F

@Temperature 77.0 - 1110 °F
Thermal Conductivity 29.8 W/m-K
207 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.010 %
0.010 %
Cobalt, Co 48.75 %
48.75 %
Iron, Fe 49 %
49 %
as remainder
Manganese, Mn 0.050 %
0.050 %
Niobium, Nb (Columbium, Cb) 0.050 %
0.050 %
Silicon, Si 0.050 %
0.050 %
Vanadium, V 1.9 %
1.9 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000400 ohm-cm
0.0000400 ohm-cm
Curie Temperature 940 °C
1720 °F