Thermal Properties Metric English Comments
Glass Transition Temp, Tg 79.0 °C
174 °F
TM R050-25
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-105C PET Bottle Grade
A co-polymer used for soft drinks and other applications.
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET F097H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET F097HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Glass Transition Temp, Tg 79.0 - 81.1 °C
174 - 178 °F
Average value: 80.0 °C Grade Count:5
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Glass Transition Temp, Tg 79.0 °C
174 °F
Eastman Eastar GN101 PETG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-101C PET Sheet Grade
A sheet grade polymer used in thick films.
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-103C PET Bottle Grade
A co-polymer used for mineral water bottles
Glass Transition Temp, Tg 79.0 °C
174 °F
Lucite International Elvacite ® 2614 Acrylic Resin
Elvacite® 2614 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial..
Glass Transition Temp, Tg 79.0 °C
174 °F
Armstrong A-31 Epoxy Adhesive
Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact..
Glass Transition Temp, Tg 79.0 °C
174 °F
Armstrong C-1/H20 Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..