Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Glass Transition Temp, Tg | 79.0 - 81.1 °C | 174 - 178 °F | Average value: 80.0 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |