Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 79.0 °C | 174 °F | TM R050-25 |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET F096H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET F096HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET F097H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Glass Transition Temp, Tg | 79.0 - 81.1 °C | 174 - 178 °F | Average value: 80.0 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | |
Lucite International Elvacite ® 2614 Acrylic Resin Elvacite® 2614 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial.. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | |
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |
|||
Glass Transition Temp, Tg | 79.0 °C | 174 °F | |
Armstrong C-1/H20 Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |