Lucite International Elvacite ® 2614 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2614 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2614 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial lacquers, aerosols, inks, and coatings for plastics. Elvacite® 2614 is softer than the methyl methacrylate grades. Elvacite® 2614 is a low odor version of Elvacite® 2013.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Particle Size 100 - 170 µm
100 - 170 µm
Viscosity Measurement 0.19 - 0.215
0.19 - 0.215
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 56000 g/mol
56000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 13
13
Tukon Hardness
Tensile Strength 11.0 MPa
1600 psi
Elongation at Break 0.50 %
0.50 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 79.0 °C
174 °F
Chemical Properties Metric English Comments
Total Acid Number 14
14
Processing Properties Metric English Comments
Moisture Content 0.35 %
0.35 %