Material Notes:
A co-polymer used for soft drinks and other applications.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.41 g/cc
1.39 - 1.41 g/cc
PEPL-10-W-21
Bulk Density 0.800 - 0.900 g/cc
0.0289 - 0.0325 lb/in³
PEPL-10-W-67
Bead Size 2.20 mm
0.0866 in
chip size, length; PEPL-10-W-71
2.60 mm
0.102 in
chip size, D2; PEPL-10-W-71
3.10 mm
0.122 in
chip size, D1; PEPL-10-W-71
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
intrinsic, [dl/gm]; PEPL-10-W-15
Molecular Weight 25500 g/mol
25500 g/mol
Number average M
51000 g/mol
51000 g/mol
Weight average M
Ash 0.025 %
0.025 %
PEPL-10-W-66
Thermal Properties Metric English Comments
Heat of Fusion <= 65.0 J/g
<= 28.0 BTU/lb
Density at 1.38 g/cc
Specific Heat Capacity 1.10 J/g-°C

@Temperature 20.0 °C
0.263 BTU/lb-°F

@Temperature 68.0 °F
1.37 J/g-°C

@Temperature 80.0 °C
0.327 BTU/lb-°F

@Temperature 176 °F
1.44 J/g-°C

@Temperature 100 °C
0.344 BTU/lb-°F

@Temperature 212 °F
1.82 J/g-°C

@Temperature 200 °C
0.435 BTU/lb-°F

@Temperature 392 °F
2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
0.242 W/m-K

@Temperature 20.0 °C
1.68 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
solid
Melting Point 248 - 250 °C
478 - 482 °F
PEPL-10-W-19
Maximum Service Temperature, Air <= 70.0 °C
<= 158 °F
Glass Transition Temp, Tg 79.0 °C
174 °F
PEPL-10-W-19
Flash Point 480 °C
896 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
when packed; PEPL-10-W-13
Descriptive Properties Value Comments
Acetaldehydes (ppm) <1
PEPL-10-W-20
Chips per Gram 60-64
PEPL-10-W-13
COOH end groups (mval/kg) <30
PEPL-10-W-16
Fines (ppm) <100
PEPL-10-W-65