Polymer Property : Glass Transition Temp, Tg = -40.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -44.0 - -40.0 °C
-47.2 - -40.0 °F
(DMA) @ 1 Hz
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -48.0 - -40.0 °C

@Frequency 1.00 Hz
-54.4 - -40.0 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Glass Transition Temp, Tg -42.0 - -40.0 °C

@Frequency 1.00 Hz
-43.6 - -40.0 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Glass Transition Temp, Tg -46.0 - -40.0 °C
-50.8 - -40.0 °F
(DMA) @ 1 Hz
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -42.0 - -40.0 °C

@Frequency 1.00 Hz
-43.6 - -40.0 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Glass Transition Temp, Tg -46.0 - -40.0 °C
-50.8 - -40.0 °F
Average value: -43.0 °C Grade Count:3
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..