Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | DMA |
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Glass Transition Temp, Tg | -44.0 - -40.0 °C | -47.2 - -40.0 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | |
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | |
Mallard Creek Polymers ROVENE® 9423 SBR Latex ROVENE® 9423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | |
Mallard Creek Polymers ROVENE® 4423 SBR Latex ROVENE® 4423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | |
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | DSC |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | 10°C/min |
Covestro Texin® 990 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | 10°C/min |
Covestro Texin® 990R Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Glass Transition Temp, Tg | -44.0 °C | -47.2 °F | DSC |
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat.. |