Polymer Property : Glass Transition Temp, Tg = -43.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -42.0 - -39.0 °C
-43.6 - -38.2 °F
(DMA) @ 1 Hz
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -42.0 - -39.0 °C
-43.6 - -38.2 °F
(DMA) @ 1 Hz
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
Mallard Creek Polymers ROVENE® 4813 SBR Emulsion
ROVENE® 4813 is a high gel content hot polymerized SBR latex with 30% bound styrene content. It has excellent shear stability and high tolerance for fillers and pH shock. It is easily tackified a..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
DSC
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
10°C/min
Covestro Texin® 285 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye..
Glass Transition Temp, Tg -42.0 - -40.0 °C

@Frequency 1.00 Hz
-43.6 - -40.0 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
10°C/min
Arkema Group Kynar® 9000 HDC N 123 PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
DSC
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer
Product Description: Exxelor VA 1801 polymer resin is a medium viscosity, semi-crystalline ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone..
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l..
Glass Transition Temp, Tg -42.0 - -40.0 °C

@Frequency 1.00 Hz
-43.6 - -40.0 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..