Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | DMA |
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | DMTA |
Lord Adhesives Thermosetâ„¢ UR-340 Two Component Urethane Encapsulant Lord UR-340 is a two component, room temperature curing, urethane encapsulating compound. It is low in viscosity and has excellent flow characteristics. Its flexibility, low modulus characteristics,.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | |
Sorbothane Polyurethane Damping Material, 30 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | DSC |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | 10°C/min |
Covestro Texin® 245 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | 10°C/min |
Covestro Texin® 985U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.. |
|||
Glass Transition Temp, Tg | -46.0 °C | -50.8 °F | 10°C/min |
Covestro Texin® 985 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Glass Transition Temp, Tg | -46.0 - -40.0 °C | -50.8 - -40.0 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -46.0 - -40.0 °C | -50.8 - -40.0 °F | Average value: -43.0 °C Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |