Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
Elongation at Break 520 %
520 %
ASTM D412
100% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
ASTM D3418
Processing Properties Metric English Comments
Processing Temperature 185 - 205 °C
365 - 401 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved