Material Notes:
General purpose neopreneInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 42
>= 42
ASTM D2240, Type A
52
52
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 10.75 MPa
>= 1559 psi
ASTM D412 Method A
14.47 MPa
2099 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 0.572 MPa
>= 83.0 psi
Stress at Elongation M50; ASTM D412 Method A
0.586 MPa
85.0 psi
AVG Stress at Elongation M25; ASTM D412 Method A
0.814 MPa
118 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 0.917 MPa
>= 133 psi
Stress at Elongation M100; ASTM D412 Method A
1.28 MPa
186 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 255 %
>= 255 %
ASTM D412 Method A
485 %
485 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.00345 GPa
0.501 ksi
ASTM D412 Method A
Shear Modulus 0.00115 GPa
0.167 ksi
ASTM D412 Method A
Secant Modulus 0.00325 GPa
0.471 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 9