Material Notes:
Al-42%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 176 MPa
25500 psi
Tensile Strength, Yield 155 MPa
22500 psi
Modulus of Elasticity 102 GPa
14800 ksi
Flexural Strength 213 MPa
30900 psi
Three Point Bend
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 25.0 - 100 °C
6.89 µin/in-°F

@Temperature 77.0 - 212 °F
13.6 µm/m-°C

@Temperature 25.0 - 200 °C
7.56 µin/in-°F

@Temperature 77.0 - 392 °F
14.4 µm/m-°C

@Temperature 25.0 - 300 °C
8.00 µin/in-°F

@Temperature 77.0 - 572 °F
15.2 µm/m-°C

@Temperature 25.0 - 500 °C
8.44 µin/in-°F

@Temperature 77.0 - 932 °F
Specific Heat Capacity 0.820 J/g-°C
0.196 BTU/lb-°F
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 58 %
58 %
Silicon, Si 42 %
42 %