Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Sapco Partially Stabilized TZP Zirconia (YSZ) Information provided by Sapco. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | DINV ENV 821-3 |
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3 MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | DINV ENV 821-3 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | DINV ENV 821-3 |
CeramTec MZ 429 Zirconia, ZrO2-Y2O3 MZ 429 is a yttria-stabilized zirconia ceramic. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | DINV ENV 821-3 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | ASTM E1269 |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | ASTM E1269 |
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | ASTM E1269 |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | E 1461-01 |
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | E 1461-01 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | Silicone Property; E1461-01 |
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | Silicone Property; E1461-01 |
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | silicone property; ASTM E 1461-1 |
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | silicone property; ASTM E 1461-1 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Specific Heat Capacity | 0.400 J/g-°C @Temperature 100 - 200 °C |
0.0956 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |