Material Notes:
Physical Properties Metric English Comments
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.0 MPa
5370 psi
Modulus of Elasticity 0.700 - 1.00 GPa
102 - 145 ksi
Compressive Strength 80.0 - 120 MPa
11600 - 17400 psi
Thermal Properties Metric English Comments
CTE, linear 10.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Specific Heat Capacity 0.400 J/g-°C
0.0956 BTU/lb-°F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00100 - 0.00300 ohm-cm
0.00100 - 0.00300 ohm-cm
Magnetic Coercive Force, Hc 5500 Oe
5500 Oe
9100 Oe
9100 Oe
Intrinsic
Magnetic Remanence, Br 6900 Gauss
6900 Gauss
Magnetic Maximum Energy Product, BH 10.5 MGOe
10.5 MGOe
Curie Temperature 300 - 470 °C
572 - 878 °F
Descriptive Properties Value Comments
Reversible Temp Coef., Bd -0.11 %/°C
Reversible Temp Coef., Hd -0.39 %/°C
Temperature Coefficient, Br -0.11 %/°C
(20-100°C)
Temperature Coefficient, Hci -0.39 %/°C
(20-100°C)