CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Corrosion: Although all Coors Ceramics are highly resistant to chemical attack, Coors recommends obtaining specific application data from Coors before design finalization.Data Provided by the manufacturer, Coors Ceramics Co.
Physical Properties Metric English Comments
Density 6.02 g/cc
0.217 lb/in³
ASTM C20
Water Absorption 0.00 %
0.00 %
ASTM C373
Particle Size 1.0 µm
1.0 µm
Average Crystal Size - Thin Section Test
Mechanical Properties Metric English Comments
Knoop Microhardness 12.7
12.7
1000 g load
Hardness, Rockwell 45 N 81
81
GPa
Modulus of Elasticity 210 GPa
30500 ksi
ASTM C848
Flexural Strength 1240 MPa
180000 psi
ASTM F417
Compressive Strength 2500 MPa
363000 psi
ASTM C773
Poissons Ratio 0.23
0.23
ASTM C848
Fracture Toughness 13.0 MPa-m½
11.8 ksi-in½
Notched Beam
Shear Modulus 85.0 GPa
12300 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 1000 °C
5.72 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.400 J/g-°C
0.0956 BTU/lb-°F
ASTM E1269
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1500 °C
2730 °F
No Load
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
ASTM D1829
<= 1000 ohm-cm

@Temperature 1000 °C
<= 1000 ohm-cm

@Temperature 1830 °F
ASTM D1829
20000 ohm-cm

@Temperature 500 °C
20000 ohm-cm

@Temperature 932 °F
ASTM D1829
Dielectric Constant 29

@Frequency 1e+6 Hz
29

@Frequency 1e+6 Hz
Dielectric Strength 9.00 kV/mm
229 kV/in
ac; ASTM D116
Dielectric Loss Index 0.0010
0.0010
at 25°C, 1 MHz; ASTM D2520
Descriptive Properties Value Comments
Color Ivory