Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 117 - 121 °C | 243 - 250 °F | |
Hong Kun Group DOPO Flame Retardant Chemical Name: 6H-DIBENZ(C,E)(1,2)OXAPHOSPHORIN-6-OXIDECAS No. 35948-25-5All information provided by Hongkun Group |
|||
Melting Point | 92.0 - 121 °C | 198 - 250 °F | |
Indium Corp. Indalloy 63 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 120 - 121 °C | 248 - 250 °F | |
Indium Corp. Indalloy 64 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 116 - 121 °C | 240 - 250 °F | ASTM D3418 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Melting Point | 105 - 121 °C | 221 - 250 °F | Average value: 112 °C Grade Count:135 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |