DuPont™ Entira® AS500 Ionomer Resin

Category Polymer , Thermoplastic , Ionomer
Manufacturer DuPont
Trade Name Entira®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Entira® AS500 Ionomer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entira™ AS MK400 is used to lower the static decay time and surface resistivity of polyolefins and other polymers. Entira™ AS MK400 can be precompounded or dry blended into polymers for extrusion, molding, or various other processing methods. Antistatic agent for use in films, moldings, and extruded forms. Entira™ AS MK400 complies with the U.S. Food and Drug Administration FDA Status Information regulation 21.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792, ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 92.0 °C
198 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 250 °C
<= 482 °F