Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 840 - 860 °C | 1540 - 1580 °F | |
Wieland 1910 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |