Goodfellow Copper 85/Silicon 15 Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Copper 85/Silicon 15 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 840 °C
1540 °F
Component Elements Properties Metric English Comments
Copper, Cu 85 %
85 %
Silicon, Si 15 %
15 %