Shandong Dongyue Polymer DF-21B PTFE Presintered Resin

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-21B PTFE Presintered Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 007-2004Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Particle Size <= 500 µm
<= 500 µm
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Descriptive Properties Value Comments
Machining Method Ram extrusion
Powder Flow (g/min) 450
Smoothness & Cleanliness First Grade: Clean and white surface, no metal impurity, the impurity quantity from 1-3 mm doesn't exceed two
Qualified: Clean and white surface, no metal impurity, the impurity quantity from 1-3 mm doesn't exceed four