Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 001-2003Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.16 g/cc
2.13 - 2.16 g/cc
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Particle Size 65 µm
65 µm
<3%
Mechanical Properties Metric English Comments
Tensile Strength >= 27.4 MPa
>= 3970 psi
Qualified
>= 29.0 MPa
>= 4210 psi
Grade A
Elongation at Break >= 280 %
>= 280 %
Qualified
>= 300 %
>= 300 %
Grade A
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
For Check Execute according to requirement of HQ/T2903-1997
For Process For Molding
Smoothness & Cleanliness Clean and white surface, even texture, total impurity quantity < 6, impurity quantity (0.5-2 mm) < 2, impurity quantity (2-3 mm) < 1
Thermal Inst. Index <20