Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 001-2003Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.16 g/cc
2.13 - 2.16 g/cc
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Particle Size 65 µm
65 µm
<3%
Mechanical Properties Metric English Comments
Tensile Strength >= 27.4 MPa
>= 3970 psi
Qualified
>= 29.0 MPa
>= 4210 psi
Grade A
Elongation at Break >= 280 %
>= 280 %
Qualified
>= 300 %
>= 300 %
Grade A
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 80.0 kV/mm
>= 2030 kV/in
Qualified
>= 100 kV/mm
>= 2540 kV/in
Grade A
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
For Check Execute according to requirement of HG/T2903-1997
For Process For Molding
Smoothness & Cleanliness White sheet surface, even texture, no contamination
Thermal Inst. Index <20