Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 980 - 2610 °C | 1800 - 4730 °F | |
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1 For arcing electrical contactsInformation provided by CMW Inc. |
|||
Melting Point | 980 - 2610 °C | 1800 - 4730 °F | |
CMW® ELKONITE® 7165 Molybdenum Silver contact material For arcing electrical contactsInformation provided by CMW Inc. |
|||
Melting Point | 980 - 2610 °C | 1800 - 4730 °F | |
CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Melting Point | 980 - 2610 °C | 1800 - 4730 °F | |
CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 2610 °C | 1980 - 4730 °F | |
CMW® THERMKON® 65M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 2610 °C | 1980 - 4730 °F | |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Melting Point | 1080 - 2610 °C | 1980 - 4730 °F | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |