CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1

Category Metal , Metal Matrix Composite , Nonferrous Metal , Molybdenum Alloy , Precious Metal , Silver Alloy , Refractory Metal
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For arcing electrical contactsInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.18 g/cc
0.3678 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 85
85
Flexural Modulus 0.931 GPa
135 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 240 W/m-K
1670 BTU-in/hr-ft²-°F
Melting Point 980 - 2610 °C
1800 - 4730 °F
Solidus 980 °C
1800 °F
Liquidus 2610 °C
4730 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 65 %
65 %
Silver, Ag 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000392 ohm-cm
0.00000392 ohm-cm
(44% IACS)