Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated

Category Metal , Metal Matrix Composite , Nonferrous Metal , Molybdenum Alloy , Precious Metal , Silver Alloy , Refractory Metal
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.23 g/cc
0.3696 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 67
67
Flexural Modulus 0.758 GPa
110 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 280 W/m-K
1940 BTU-in/hr-ft²-°F
Melting Point 980 - 2610 °C
1800 - 4730 °F
Solidus 980 °C
1800 °F
Liquidus 2610 °C
4730 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 50 %
50 %
Silver, Ag 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000370 ohm-cm
0.00000370 ohm-cm
(55% IACS)
Users viewing this material also viewed the following: