Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 201 °C | 394 °F | ASTM D789 |
NYCOA 2366 Plasticized Copolyamide TPE NYCOA 2366 is an extremely flexible and transparent Nylon copolymer specifically developed for extrusion applications such as high-end fishing line, and flexible tubing. NYCOA 2366 possesses an extr.. |
|||
Melting Point | 201 °C | 394 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Melting Point | 201 - 211 °C | 394 - 412 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Melting Point | 201 °C | 394 °F | ASTM D3418 |
SK Chemicals SKYPEL M555CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 201 °C | 394 °F | ISO 3146 |
Chengdu Polyster FH605 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H605 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by .. |
|||
Melting Point | <= 201 °C | <= 394 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide .. |
|||
Melting Point | <= 201 °C | <= 394 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 10.. |
|||
Melting Point | 201 °C | 394 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Melting Point | 201 °C | 394 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® PC956 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Melting Point | 201 °C | 394 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® SC956 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Melting Point | 201 °C | 394 °F | ASTM D3418 |
ALM PA 860 White Nylon 11 SLS Prototyping Polymer Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod.. |
|||
Melting Point | <= 201 °C | <= 394 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 705.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 705.MJ is a fractional melt index, 12.8 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and.. |