NYCOA 2366 Plasticized Copolyamide TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Nylon
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 2366 Plasticized Copolyamide TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCOA 2366 is an extremely flexible and transparent Nylon copolymer specifically developed for extrusion applications such as high-end fishing line, and flexible tubing. NYCOA 2366 possesses an extremely high degree of softness, flexibility, and transparency compared to standard monofilament grade nylons. NYCOA 2366 can be easily extruded on most equipment. This product is available in heat and light stable grades.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.7 %
1.7 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Strength 14.0 MPa
2030 psi
ASTM D790
Flexural Modulus 0.250 GPa
36.3 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 201 °C
394 °F
ASTM D789
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified