Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 188 °C | 370 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Melting Point | 188 °C | 370 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The .. |
|||
Melting Point | 188 - 204 °C | 370 - 399 °F | TMA Melt Range |
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers |
|||
Melting Point | 188 - 198 °C | 370 - 388 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r.. |
|||
Melting Point | 188 °C | 370 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® CI 31 F 000000 Copolyamide PA6/6I Copolyamide PA6/6I, low melt point (188-191°C), low viscosity, no additives, very high transparency, in compliance with FDA as far as the PA-layer is separated from the food by a 50 µm PE film.. |
|||
Melting Point | 188 °C | 370 °F | peak; 0.025" extruded film |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |