Polymer Property : Melting Point = 204 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 188 - 204 °C
370 - 399 °F
TMA Melt Range
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers
Melting Point 196 - 204 °C
385 - 400 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer
PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist..
Melting Point 134 - 204 °C
272 - 399 °F
Average value: 161 °C Grade Count:80
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..