Thermal Properties Metric English Comments
Melting Point 151 °C
304 °F
Flow temperature, ASTM D569-59
Rotuba 860MH 686.4 Ethyl Cellulose
Data provided by the manufacturer.
Melting Point 151 °C
304 °F
DSC
Silon Tabond 5007 Adhesive Resin
Tabond 5007 is a chemically modified Polypropylene. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion to aminosi..
Melting Point 151 °C
304 °F
ISO 3146
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene
ATOFINA Polypropylene MR 2001 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w..
Melting Point 151 °C
304 °F
ISO 3146
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene
ATOFINA Polypropylene MR 2002 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w..
Melting Point 151 °C
304 °F
DSC
Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade
M3766 is an isostatic form of polypropylene made via TOTAL proprietary technology.Recommended Applications. M3766 is recommended for melt spun and spun bound fiber applications. However, due to it..
Melting Point 151 °C
304 °F
DSC
Total PPH M3865 Metallocene Isostatic Propylene Polymer, Fiber Grade
M3865 is an isostatic form of polypropylene made via ATOFINA proprietary technology.Recommended Applications. M3865 is recommended for melt spun and spunbond fiber applications. However, due to it..
Melting Point <= 151 °C
<= 304 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer
Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends..
Melting Point 151 - 155 °C
304 - 311 °F
Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Melting Point 151 °C
304 °F
DSC
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene
OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA..