Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax BlendsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ExxonMobil method
Vinyl Acetate Content 27.6 %
27.6 %
ExxonMobil method
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 77

@Time 15.0 sec
77

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 22

@Time 15.0 sec
22

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 2.90 MPa
420 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus, 1% Secant 18.6 MPa
2700 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 151 °C
<= 304 °F
Peak Melting Point; ExxonMobil method
Copyright © lookpolymers.com All Rights Reserved