Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
M3766 is an isostatic form of polypropylene made via TOTAL proprietary technology.Recommended Applications. M3766 is recommended for melt spun and spun bound fiber applications. However, due to its unique and interesting properties, other applications may exist.Processing. M3766 is a narrower molecular weight distribution product that conventional polypropylene.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 23 g/10 min
23 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Yield 185 %
185 %
ASTM D3218
Tenacity 0.221 N/tex
2.50 g/denier
ASTM D3218
Thermal Properties Metric English Comments
Melting Point 151 °C
304 °F
DSC
Descriptive Properties Value Comments
Xylene Solubles 0.7 to 1.2