Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 60.0 °C | 140 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin
(discontinued **) Enable EN 33900 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical |
|||
Melting Point | 60.0 - 70.0 °C | 140 - 158 °F | |
Fine Organics FINALUX G 471 Lubricant Additive Applications: Intermediate lubricant suggested for rigid PVC processing especially extrusion.Information provided by Fine Organics |
|||
Melting Point | 60.0 °C | 140 °F | Eutectic |
Indium Corp. Indalloy® 19 In-Bi-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 60.0 - 70.0 °C | 140 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 106 Linear Thermoplastic Polyurethane Pearlbond™ 106.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a very high thermoplasticity l.. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melting Point | 60.0 - 130 °C | 140 - 266 °F | |
Lucobit Lucowax® 1700 Polyethylene Wax Lucowax is a polyethylene wax additive for the modification of bitumen or asphalt.The addition of Lucowax reduces viscosity and penetration, while increasing water resistance, plasticity, and deform.. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane Pearlbond™ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane Pearlbond™ 503 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melting Point | 60.0 - 65.0 °C | 140 - 149 °F | RP-0815 |
Solvay ALKAMIDE® C 212 Surfactant INCI NAME: Cocamide MEACAS: 68140-00-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMIDE C-212 is a versatile and effective alkanolamide for use in soap or syn.. |
|||
Melting Point | >= 60.0 °C | >= 140 °F | GB4608 |
Suzhou Hipro Polymers Hipromin® 102 1.10 Decamethylenediamine Hipromin® 102 (1.10-Decamethylenediamine) is widely used for long chain polyamide polymerization, molecular weight regulation, cross linking, etc.Information provided by Suzhou Hipro Polymers Co... |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8100 Polyolefin Elastomer Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap.. |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8107 Polyolefin Elastomer Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8200 Polyolefin Elastomer Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermo.. |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8207 Polyolefin Elastomer Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8400 Polyolefin Elastomer Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr.. |
|||
Melting Point | 60.0 °C | 140 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8407 Polyolefin Elastomer Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p.. |
|||
Melting Point | 60.0 - 65.0 °C | 140 - 149 °F | |
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Melting Point | 60.0 °C | 140 °F | Freezing Point; ASTM D3417, ISO 3146 |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Melting Point | 60.0 - 109 °C | 140 - 228 °F | Average value: 87.4 °C Grade Count:12 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I.. |
|||
Melting Point | 60.0 °C | 140 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Melting Point | 60.0 °C | 140 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® CM3326 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM3326 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low.. |