Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7189 PC Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East) Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl EN130S PPE+HIPS (Europe-Africa-Middle East) Noryl EN130S is an extrusion grade with a Vicat B/120 temperature of 140 deg C, developed for profile extrusion and in compliance with Food contact regulations; color limited.This data was supplied .. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV6 220 PBT-GF10 10% Glass Reinforced |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® FR6901 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Hig.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® 1010N2 1ES NAT PA6 FR(30) Injection Molding, Flame Retardant (Halogen free) |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 30 LS nat PA* Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing a.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 30 nat PA* Product description: Grilamid TR 30 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 natural offers outstanding properties.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LE 6010 HV Nylon Alloy, 10% Glass Fiber Reinforced (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents). 10% glass fiber reinforced. Suited to blow molding of technical pa.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral
(discontinued **) PBT, 30% mineral, injection molding, LDS |