EMS-Grivory Grivory® AS V0 PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® AS V0 PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-freeLight natural colorUL 94 V-0 at 0.75 mm wall thicknessGood electrical properties Grilon AS V0 is used typically for contact plates, plugs, buttons, plug-in terminal strips, switch components.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 55.0 MPa
7980 psi
conditioned; ISO 527-1/-2
90.0 MPa
13100 psi
dry; ISO 527-1/-2
Elongation at Break 9.0 %
9.0 %
dry; ISO 527-1/-2
9.0 %
9.0 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.00 GPa
290 ksi
conditioned; ISO 527-1/-2
3.90 GPa
566 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 32 %
32 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
dry; IEC 60250
4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
dry; IEC 60250
4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
conditioned; IEC 60250
7.0

@Frequency 100 Hz
7.0

@Frequency 100 Hz
conditioned; IEC 60250
Dielectric Strength 28.0 kV/mm
711 kV/in
conditioned; IEC 60243-1
31.0 kV/mm
787 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Cables & Tubes
Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Form Granules
Processing Injection Molding
Special Characteristics Flame retardant